The purpose of mounting is to protect fragile or coated materials during the preparation and to obtain good edge retention. Mounting is also used to produce specimens with uniform size. Two different techniques are available: hot mounting and cold mounting.
Struers mounting presses use low-mass heating/cooling system allowing for rapid heat transfer and faster cooling. In addition, water consumption can be reduced by 80% with Struers pulsed-cooling system.