Paint Layer Challenge

Manual grinding and polishing is difficult to control and therefore includes a high risk of grinding away the subject for the examination. Targets can be invisible on the surface of the sample.

Solution

A reproducible method for evaluation of paint defects was developed consisting of:

  • Precision cutting with Accutom-100 to isolate the point of interest in distance of µm
  • Mounting and alligning the sample in special holder, Target Grip, 
  • Controlled Material Removal (CMR) with TargetMaster in a 5 step method reaching the paint defect in 12,5 minutes

Tell us who you are and you may download a materialographic solution report of one of our many method solutions. Please don’t hesitate to contact us if you have a specific problem that you would like us to help you with 