LectroPol

Save time when polishing and etching with the automatic, microprocesser-controlled LectroPol-5 electrolytic polishing machine

LectroPol-5 facts

  • Scanning function
  • Method database
  • Easy to use
  • Maximum reproducibility

The LectroPol-5 is designed for automated electrolytic polishing and etching of metallographic specimens. A scanning function for easy determination of parameters, built-in safety features, and a database with methods for various materials enables short polishing times and maximum reproducibility.

LectroPol-5 consists of two units, the control unit and the polishing unit. The two units can be separated from each other.

Contact

Automatic determination of parameters

LectroPol-5 features a scanning function that helps to determine the correct voltage for both polishing and etching, thus saving time and avoiding human error. LectroPol-5 displays the scan curve, while the user selects and sets the voltage. Instead of time-consuming trial and error parameter testing is now easy to find the correct settings after a single scan of a new sample material.

Method database

The LectroPol-5 comes with 10 polishing/etching methods for various materials, enabling immediate preparation of a wide range of materials without any lengthy and time-consuming trials. These methods can also be used as starting points for the development of methods for other materials. The LectroPol-5 database can store 20 user-defined methods.

Short polishing times and high reproducibility

Electrolytic polishing and etching have very short preparation times compared with normal mechanical specimen preparation. Microprocessor control and database functions ensure the use of correct parameters. LectroPol- 5 combines both short preparation times and high reproducibility and is thus the ideal choice for fast quality control requirements.

KEY FEATURES THAT ENSURE CORRECT PREPARATION AND INSPECTION

  • LectroPol control unit

    The control unit

    Both the power supply and the programming and monitoring functions are incorporated in the control unit. Easy touchpad operation combines with a back-lit graphic display of all parameters and monitoring of the process.

    The control unit
  • LectroPol polishing above

    Polishing

    The separate unit design enables the polishing unit to be placed away from the control unit, for example in a fume cabinet. The process can also be started directly from the polishing unit. The electrolyte is stored in easily exchangeable electrolyte containers that are inserted into the polishing unit.

    Polishing
  • LectroPol  safety

    Built-in safety features

    All functions are controlled using advanced software. An increase in the electrolyte temperature above a pre-defined limit will automatically result in either a warning or shut-down of the procedure in progress. Voltage and current are constantly monitored and settings are automatically kept within the limits of Lectro-Pol-5.

    Built-in safety features
  • LectroPol advanced cooling

    Advanced cooling control

    LectroPol-5 features a built-in measuring and control system that constantly monitors the electrolyte temperature. If the temperature exceeds the given limit, water is run through the cooling coil. If no water is connected, or the electrolyte temperature continues to rise, a warning is displayed and the LectroPol-5 automatically shuts down.

    Advanced cooling control
  • LectroPol polishing below

    Polishing at below freezing

    A special LectroPol polishing unit is used for this application. Stainless steel cooling coils are led directly to the back of the polishing unit where they can be connected to an external cooling unit. The external cooling unit takes over temperature control and regulation of the electrolyte, enabling materials to be polished at sub-zero temperatures.

    Polishing at below freezing
  • LectroPol  etching

    External etching

    LectroPol-5 can also be used for external etching (controlled by a preset voltage exposure and polishing time)

    External etching

Facts

Model types

LectroPol-5

LectroPol electrolytic polishing machine
LectroPol-5
Fully automatic, microprocessor controlled electrolytic polishing and etching apparatus. Complete with control unit, polishing unit and external etching unit. One set of masks and two electrolyte containers included.


Lorem ipsum dolor sit amet, consectetuer adipiscing elit, sed diam nonummy nibh euismod tincidunt ut laoreet dolore magna aliquam erat volutpat. Ut wisi enim ad minim veniam, quis nostrud exerci tation ullamcorper suscipit lobortis nisl ut aliquip ex ea commodo consequat. Duis autem vel eum iriure dolor in hendrerit in vulputate velit esse molestie consequat, vel illum dolore eu feugiat nulla facilisis at vero eros et accumsan et iusto odio dignissim qui blandit praesent luptatum zzril delenit augue duis dolore te feugait nulla facilisi


Lorem ipsum dolor sit amet, consectetuer adipiscing elit, sed diam nonummy nibh euismod tincidunt ut laoreet dolore magna aliquam erat volutpat. Ut wisi enim ad minim veniam, quis nostrud exerci tation ullamcorper suscipit lobortis nisl ut aliquip ex ea commodo consequat. Duis autem vel eum iriure dolor in hendrerit in vulputate velit esse molestie consequat, vel illum dolore eu feugiat nulla facilisis at vero eros et accumsan et iusto odio dignissim qui blandit praesent luptatum zzril delenit augue duis dolore te feugait nulla facilisi

Struers’ equipment is in conformity with the provisions of the applicable International Directives and their appurtenant Standards.
Struers’ products are subject to constant product development. Therefore, we reserve the right to introduce changes in our products without notice.

Technical Data

LectroPol Technical Data Sheet

Struers Technical Data Sheets are designed to help you make the best choice of equipment for your particular purpose. You can find important information such as capacity and performance specifications, dimensions, weight, electrical data, noise levels, ambient conditions and safety. In many cases you can also obtain an overview of accessories offering higher capacity and performance.

Download Technical Data Sheet
Technical Data Sheet

Application specialists

The fast track to expert knowledge…

Correct preparation solutions

True structures require proper correct applications. Different material properties require broad application knowledge. Struers Application Specialists are experts in optimising preparation methods, because application knowledge is necessary to select the correct preparation solutions. Your material – our application solutions.

Birgitte Nielsen
Application Specialist, Struers ApS

Go to Knowledge

M8 Quote Birgitte

MEET SOME OF OUR CUSTOMERS

Don’t make do with what we say! Look for the truth in the experiences of the people who use our equipment and knowledge. We asked a few of our loyal customers to tell us what they think is most important about Struers.

John Crane Logo
We have been using Struers equipment and consumables for almost 30 years and have benefitted enormously from their unparalleled service and applications support. John Crane UK Ltd. (UK) Bill Taylor Materials & Forensics Engineer
Nissan Logo
Since adopting Struers equipment, we made significant savings within our manufacturing process as a result of reduced manpower requirements and productivity improvements. Nissan Motor Manufacturing UK Ltd. John Smart Production Supervisor
WWU Münster Institut für Planetologie Logo
My relations with Struers date back over many years. The reason is their competent advice, the good service and their use of our application laboratory in the case of difficult questions that are best resolved on-site. WWU Münster, Institut für Planetologie Ursula Heitmann Mineral Specimen Preparer