The MD-System is a comprehensive line of grinding discs and polishing cloths with metallic backings available in 200 mm / 8-inch, 250 mm / 10-inch and 300 mm /12-inch diameters.
A single magnetic platen, positioned on the grinding and polishing machine throughout the preparation process, is used to support the new preparation surfaces. In addition to cost and time savings, the new method eliminates the storage, handling complications and disposal of SiC papers.
The grinding discs in the MD-System makes it possible to reduce the typical grinding process involving SiC-Paper to just two steps, and cut total preparation time. The preparation quality is tremendously improved compared to SiC-Paper. Thus, the grinding discs in the MD-System are superior to SiC-Paper regarding both pre-performances.
Because the specimens are totally flat after the first grinding step on MD-Piano, the time on the following fine grinding step on MD-Allegro can be reduced by about 50%.
The succeeding polishing steps can also be carried out in a shorter time because of the outstanding planeness achieved in the fine grinding step.
More Information