DESCRIPTION:After sectioning the sample\, the lab technician must use
a series of grinding and polishing steps to remove deformation and cracks
to expose the true microstructure. After mechanical preparation\, the sam
ple should be scratch-free\, free from deformation\, and ready for the mic
roscope or hardness tester! Please join us as we discuss the basics of gri
nding and polishing sample materials. We will also discuss tips and tricks
to solve some common preparation issues.
\n
\nThis webinar will cover:
\n
\n&bull\; Types of abrasives used for grinding and
polishing
\n&bull\; Choosing preparation surfaces based on material\n&bull\; H
ow to adjust common preparation parameters\, like force\, rpm\, dosing\, a
nd time
\
n&bull\; Water-free preparation for water-sensitive materials
\n&bull\;
Tips and tricks for common preparation problems<\;/span">\;
DTEND:20200428T190000Z
DTSTAMP:20240328T154809Z
DTSTART:20200428T180000Z
LOCATION:
SEQUENCE:0
SUMMARY:Grinding and Polishing of Sample Materials for Microstructural Anal
ysis and Hardness Testing
UID:acd848d0-abc7-430b-8ee3-2c1983016180
X-ALT-DESC;FMTTYPE=text/html:After sectioning the sample\, the lab te
chnician must use a series of grinding and polishing steps to remove defor
mation and cracks to expose the true microstructure. After mechanical prep
aration\, the sample should be scratch-free\, free from deformation\, and
ready for the microscope or hardness tester! Please join us as we discuss
the basics of grinding and polishing sample materials. We will also discus
s tips and tricks to solve some common preparation issues.
\n
\nThis webinar will cover:
\n
\n&bull\; Types of abrasives used
for grinding and polishing
\n&bull\; Choosing preparation surfaces based on
material
\n&bull\; How to adjust common preparation parameters\, like force\,
rpm\, dosing\, and time
\n&bull\; Water-free preparation for water-sensitive
materials
\n&bull\; Tips and tricks for common preparation problems&l
t\;/span">\;