THE GEAR CHALLENGE

Learn how to prepare and test surface hardening on heat-treated helical gears using an automated and reproducible process.

Gear
Gear

Solution

Using highly-automated equipment and special clamping methods for cutting, it is possible to avoid pinching of the cut-off wheel and conduct a successive hardness tests on even the most difficult gear surfaces in a process consisting of:

  • Cutting with a Axitom-5 using special clamping methods
  • Grinding and polishing with an AbraPol-30 in 4 automated steps using a specific selected sequence of surfaces
  • A fully automated CHD-measurement of 15 indentations with Duramin-40AC1

Tell us who you are and you may download a materialographic solution report of one of our many method solutions. Please don’t hesitate to contact us if you have a specific problem that you would like us to help you with.