Butt Weld of Pure Copper

image

Submitter's Comments on the Structure:

One can clearly see grain growth in the HAZ and epitactic grain crystallization in the fusion zone.

10% iron(III)nitrate solution
Mag. 50 X

 

Preparation Equipment We Recommend to Achieve This Surface:

image

Secotom

  • Cutting capacity 50 x 165 mm.
  • Automatic precision cutting machine
  • Cut-off wheel size 75 – 203 mm/ 3- 8” dia.
The very first Secotom precision cutting machine was launched in 2001 and became an immediate success. Since then, thousands of Secotoms have left our production to serve laboratories worldwide. An intuitive user interface means that hardly any training is required. The optional automatic X-movement supersedes time-wasting re-positioning, and a movable T-slot table allows for sectioning a range of sizes and shapes. Secotom contains multiple additional features such as a laser light, an ExciCut mode for hard materials, and intelligent feed control.
Read more
image

CitoPress mounting press

  • Fastest hot mounting solution: 3.5 min. w/ CitoFast resin
  • Thousands of installations worldwide prove durability under heavy loads
  • Automatic dosing system for safer resin filling & less spillage

CitoPress is a high-performance hot mounting press designed for rapid operation and ease of use, ensuring faster turnaround times and higher productivity. The unique automatic dosing system reduces time spent on mounting by dispensing a preset amount of resin. Furthermore, it minimizes exposure to resin dust and reduces the risk of errors.

CitoPress-30
CitoPress-30 is an advanced & programmable dual cylinder mounting press that offers total process control, database facilities, and synchronous or independent operation of both cylinders.

CitoPress-15
CitoPress-15 is an advanced & programmable single cylinder mounting press, offering total process control and database facilities.

CitoPress-5
A single cylinder mounting press.

Read more
image

Tegramin

  • Semi-automatic all-purpose grinding and polishing machine
  • Advanced dosing functions for high reproducibility
  • Fine-tune multiple features for higher efficiency across different tasks

Tegramin’s compact design, integrated specimen mover, automated process control, and user-friendly operation make it a reliable, all-purpose grinding and polishing solution that delivers highly reproducible results and better process standardization. Extremely efficient, accurate, and versatile, it is ideal for labs that prepare different materials and need to adjust parameters often. Everything is designed to utilize the preparation surface area, making your consumables last longer.

Read more
image

Experience Our Equipment in Action

Discover how our solution can help streamline your lab workflows and deliver measurable results.

  • Customized demo focused on your preparation challenges
  • Discover practical solutions to improve accuracy and efficiency
  • Get insights and recommendations from our experts
Book Your Demo

Submitted by: Gaby Ketzer-Raichle, Germany

Gaby Ketzer-Raichle is a trained metallographer (Max-Planck-Institute for Metal Research in Stuttgart) and has about 40 years of experience in the application and teaching of metallography in industry and research. 
Since 2014, she has been working at Aalen University in the Institute for Materials Research. She is author of some publications in the “Practical Metallography” and, together with Prof. H. Oettel, editor of the well-known book “Schumann Metallographie.”

Consumables We Recommend to Achieve This Preparation Result:

image

We Recommend This Preparation Method:

Non Ferrous Metals Ductile (B1)

Explore the metallography method our application specialists recommend for this type of material.

Learn how to prepare your own sample