Low Carbon Steel Ferritic Microstructure

Submitter's Comments on the Structure:
Ferritic microstructure with pearlite and tertiary cementite at the grain boundaries, as well as impurities.
Klemm I
Mag. 500 X
Preparation Equipment We Recommend to Achieve This Surface:

Labotom
- Cutting capacity: 62 x 250 mm / 2.5" x 9.8"
- Manual machine with simple 3-button control panel
- Cut-off wheel size 250 mm or 350 mm / 10.0” or 14.0” dia.

CitoPress mounting press
- Fastest hot mounting solution: 3.5 min. w/ CitoFast resin
- Thousands of installations worldwide prove durability under heavy loads
- Automatic dosing system for safer resin filling & less spillage
CitoPress is a high-performance hot mounting press designed for rapid operation and ease of use, ensuring faster turnaround times and higher productivity. The unique automatic dosing system reduces time spent on mounting by dispensing a preset amount of resin. Furthermore, it minimizes exposure to resin dust and reduces the risk of errors.
CitoPress-30
CitoPress-30 is an advanced & programmable dual cylinder mounting press that offers total process control, database facilities, and synchronous or independent operation of both cylinders.
CitoPress-15
CitoPress-15 is an advanced & programmable single cylinder mounting press, offering total process control and database facilities.
CitoPress-5
A single cylinder mounting press.

Tegramin
- Semi-automatic all-purpose grinding and polishing machine
- Advanced dosing functions for high reproducibility
- Fine-tune multiple features for higher efficiency across different tasks
Tegramin’s compact design, integrated specimen mover, automated process control, and user-friendly operation make it a reliable, all-purpose grinding and polishing solution that delivers highly reproducible results and better process standardization. Extremely efficient, accurate, and versatile, it is ideal for labs that prepare different materials and need to adjust parameters often. Everything is designed to utilize the preparation surface area, making your consumables last longer.

Experience Our Equipment in Action
Discover how our solution can help streamline your lab workflows and deliver measurable results.
- Customized demo focused on your preparation challenges
- Discover practical solutions to improve accuracy and efficiency
- Get insights and recommendations from our experts
Submitted by: Jörg Hossbach, Germany
Jörg Hossbach is a trained materials tester and serves as Head of the Metallography Laboratory at SLV Halle GmbH (Welding Research and Training Institute). His passion for metallography began during his vocational training and has remained the driving force throughout his career. He is particularly fascinated by the challenges of specimen preparation, where every sample presents unique characteristics and often requires tailored preparation methods to achieve optimal results. Equally compelling to him is the study of microstructures, as each specimen reveals its own distinctive features under the microscope. This enduring curiosity frequently leads him to spend hours examining and interpreting metallographic structures.
Following his qualification as a materials tester, Jörg built extensive expertise across welding technology, failure analysis, and steel construction. Over the years, he further broadened and deepened his knowledge through professional roles in the automotive industry, gaining valuable experience in the characterization and evaluation of metallic materials. Today, he combines decades of practical and technical expertise with a continued enthusiasm for metallography, leading laboratory activities that support materials testing, welding research, and metallographic analysis.
Consumables We Recommend to Achieve This Preparation Result:

We Recommend This Preparation Method:
Ferrous Metals Soft to Medium-Hard (C2)
Explore the metallography method our application specialists recommend for this type of material.