Titanium Alloy Substrate (Ti-6Al-4V) Protected with a Ceramic Coating (TBC)

image

Submitter's Comments on the Structure:


The optical microscopy image reveals the complex microstructure of a metastable phase in the titanium alloy Ti-6Al-4V, observed after the material was subjected to a thermal ablation test. Ti-6Al-4V is widely used as a structural substrate in aerospace applications, including turbine components, and is frequently combined with thermal barrier coatings (TBCs) to extend service life under extreme thermal conditions.

Kroll’s reagent (3 ml HF, 6 ml HNO3 and 100 ml distilled H2O)
Mag. 500 X

 

Preparation Equipment We Recommend to Achieve This Surface:

image

Minitom

  • Workpieces up to 30 x 40 mm
  • High-precision tabletop machine
  • Low speed protects against heat deformation
A small, low-speed, automatic precision cutting machine for sectioning delicate materialographic workpieces that can’t tolerate the heat generated by high-speed cutting. The gravity feed design allows for sectioning of various material types, with high accuracy and reproducibility. Minitom is designed with speed and efficiency in mind. The simple design means it only takes a few minutes to setup a cut, and the machine can be set to stop automatically once the cut is done, giving you more time to work on other tasks.
Read more
image

CitoPress mounting press

  • Fastest hot mounting solution: 3.5 min. w/ CitoFast resin
  • Thousands of installations worldwide prove durability under heavy loads
  • Automatic dosing system for safer resin filling & less spillage

CitoPress is a high-performance hot mounting press designed for rapid operation and ease of use, ensuring faster turnaround times and higher productivity. The unique automatic dosing system reduces time spent on mounting by dispensing a preset amount of resin. Furthermore, it minimizes exposure to resin dust and reduces the risk of errors.

CitoPress-30
CitoPress-30 is an advanced & programmable dual cylinder mounting press that offers total process control, database facilities, and synchronous or independent operation of both cylinders.

CitoPress-15
CitoPress-15 is an advanced & programmable single cylinder mounting press, offering total process control and database facilities.

CitoPress-5
A single cylinder mounting press.

Read more
image

Tegramin

  • Semi-automatic all-purpose grinding and polishing machine
  • Advanced dosing functions for high reproducibility
  • Fine-tune multiple features for higher efficiency across different tasks

Tegramin’s compact design, integrated specimen mover, automated process control, and user-friendly operation make it a reliable, all-purpose grinding and polishing solution that delivers highly reproducible results and better process standardization. Extremely efficient, accurate, and versatile, it is ideal for labs that prepare different materials and need to adjust parameters often. Everything is designed to utilize the preparation surface area, making your consumables last longer.

Read more
image

Experience Our Equipment in Action

Discover how our solution can help streamline your lab workflows and deliver measurable results.

  • Customized demo focused on your preparation challenges
  • Discover practical solutions to improve accuracy and efficiency
  • Get insights and recommendations from our experts
Book Your Demo

Submitted by: Danieli Reis, Brazil

Dr. Danieli Reis is an Associate Professor of Metallic Materials Engineering at the Institute of Science and Technology, Federal University of São Paulo (UNIFESP), São José dos Campos campus, Brazil, where she coordinates the Mechanical Behavior of Metals Laboratory (LCMM).
She specializes in the mechanical behavior and microstructural evaluation of metallic alloys for aerospace, structural, and automotive applications, including tensile, fatigue, creep, and fracture analyses. Her research also addresses thermal barrier and oxidation-resistant coatings, surface treatments, heat treatments, and surface modification techniques for advanced and strategic materials in the aerospace and defense sectors. In 2027, the LCMM will celebrate its 20th anniversary, marking two decades of research and characterization of metallic materials in areas such as thermal barrier coatings and the creep behavior of aerospace alloys.

Consumables We Recommend to Achieve This Preparation Result:

image

We Recommend This Preparation Method:

Non Ferrous Metals Very Ductile (B2)

Explore the metallography method our application specialists recommend for this type of material.

Learn how to prepare your own sample