Product Description

Aluminium oxide grinding stone, for fast plane grinding of nickel -based alloys (turbine blades) and stainless steels on AbraPlan and MAPS.
Aluminium oxide grinding stone, for fast plane grinding of nickel -based alloys (turbine blades) and stainless steels on AbraPlan and MAPS.