Replication system. General-purpose material. Particularly useful for replicating horizontal or sloping surfaces in normal or high temperature conditions. Fluid fast curing compound with working life of 5 min. and curing time of 18 min. at 25° C. Dispensing gun (40900066) and static-mixing nozzles (40900088) are ordered separately