Replication system. Particularly useful for replicating vertical or overhead surfaces in low temperature conditions or where rapid results are required. Thixotropic rapid curing compound with working life of 0.5 - 1 min. and curing time of 4 min. at 25° C. Dispensing gun (40900066) and static-mixing nozzles (40900088) are ordered separately