Replication system especially for comparator macroscopy and metrology. Particularly useful for replicating horizontal or sloping surfaces and filling holes. Fluid rapid curing compound with working life of 0.5 - 1 min. and curing time of 4 min. at 25° C. Dispensing gun (40900066) and static-mixing nozzles (40900088) are ordered separately
Replication system especially for comparator macroscopy and metrology. Particularly useful for replicating horizontal or sloping surfaces and filling holes. Fluid rapid curing compound with working life of 0.5 - 1 min. and curing time of 4 min. at 25° C. Dispensing gun (40900066) and static-mixing nozzles (40900088) are ordered separately