Opis produktu

To be mixed with ProntoFix Hardener. 1 l resin corresponds to 275 ml hardener. If curing time with the ProntoFix Hardener is too long the ProntoFix Accelerator can be added. 1.3 l Resin corresponds to 275 ml hardener plus 70 ml accelerator
To be mixed with ProntoFix Hardener. 1 l resin corresponds to 275 ml hardener. If curing time with the ProntoFix Hardener is too long the ProntoFix Accelerator can be added. 1.3 l Resin corresponds to 275 ml hardener plus 70 ml accelerator