Duramin-600

Robust and automatic universal hardness testing

Duramin-600 – Semi-Automatic Universal Tester

  • Methods: Vickers, Knoop, Brinell and Rockwell hardness testing
  • Load ranges: 1-250 kgf, 3-750 kgf, 5-3000 kgf
  • Semi-automatic universal tester
  • Robust load cell-based universal tester
  • Automatic six-position turret
  • Ring-light with dark field illumination for the testing of soft metals
  • Optional motorized Z-axis for large samples
  • Embedded PC, operated by mouse or touchscreen
Duramin-600 is designed to survive the toughest production environment. It is a universal hardness tester, operated by a robust touchscreen, and comes available in three load ranges and with an optional motorized Z-table for larger samples.

Perfected for the production environment

Designed to last, the Duramin-600 employs industry strength components from the 400 kg frame to the display.

Easy to operate

Simple clamping, combined with clean software and a touchscreen, ensure stress-free operating and result reporting.

High accuracy

The accurate and repeatable loading system based on load cell technology, combined with advanced software algorithms, ensures specific and repeatable image and hardness evaluation.
image
High accuracy
image
Perfected for the production environment
image
Easy to operate
image
High accuracy
image
Perfected for the production environment

Facts

Model Types

The Duramin-600 models come with a motorized, six-position turret, automatic illumination adjustment, auto focus, and automatic image evaluation as standard. The maximum sample height is 330 mm, with a throat depth of 260 mm. Duramin-600 is operated via a 15-inch color touchscreen. Objective lenses and indenters are ordered separately. All Duramin-600 M models come with manual Z-axis adjustment. All Duramin-600 Z models come with a motorized Z-axis adjustment.

image

Duramin-600 M1

Universal hardness tester with load cell technology for the automatic hardness testing of Brinell, Vickers, Rockwell, and Knoop With an extended load range of 9.8 N to 2450 N (1-250 kgf).
image

Duramin-600 M2

Universal hardness tester with load cell technology for the automatic hardness testing of Brinell, Vickers, Rockwell, and Knoop With an extended load range of 29.4 N to 7,360 N (3.0-750 kgf)
image

Duramin-600 M3

Universal hardness tester with load cell technology for the automatic hardness testing of Brinell, Vickers, Rockwell, and Knoop With an extended load range of 49.1 N to 29,430 N (5.0-3,000 kgf)

Duramin-600 Z2
Universal hardness tester with load cell technology for the automatic hardness testing of Brinell, Vickers, Rockwell, and Knoop With an extended load range of 29.4 N to 7,360 N (3.0-750 kgf)

image

Duramin-600 Z1

Universal hardness tester with load cell technology for the automatic hardness testing of Brinell, Vickers, Rockwell, and Knoop With an extended load range of 9.8 N to 2450 N (1-250 kgf).                

Duramin-600 Z3
Universal hardness tester with load cell technology for the automatic hardness testing of Brinell, Vickers, Rockwell, and Knoop With an extended load range of 49.1 N to 29,430 N (5.0-3,000 kgf)