Skip to content
单价

登录以查看价格

产品描述

For cutting of soft ferrous metals, steel tubes and small pieces (HV 80 - 400) on Unitom (2.775 rpm) and Axitom (1.950 rpm), and for cutting of medium soft ferrous metals (
For cutting of soft ferrous metals, steel tubes and small pieces (HV 80 - 400) on Unitom (2.775 rpm) and Axitom (1.950 rpm), and for cutting of medium soft ferrous metals (