World’s fastest mounting process


When using Struers’ hot mounting press CitoPress together with the hot mounting resin CitoFast you’ll get the fastest mounting process on the market.
A 30 mm diameter mount with 0.45 % carbon steel specimen (20 volume%) can be processed with 2½ min heating time and 1 min cooling time, in total only 3½ minutes!

   CitoFast is ideal for mounting specimens of soft to very soft materials because of the aluminium filler.
 

   When using CitoFast as a backing resin (1/3 DuroFast/LevoFast around the specimen for special requirements and 2/3 CitoFast) you get the same fast process times as when using only CitoFast.
 