Metallographic preparation of nitrided and nitrocarburised components


   Metallography of nitrided and nitrocarburised components is mainly used for controlling the nitriding process through examination of the layer. The white layer, diffusion zone and porous zone are measured and evaluated. In addition, failure analyses of used parts are carried out to see if faulty material, surface deterioration or the nitriding process were contributing factors.
 

Download PDF (595 KB)

Struers Application Notes are designed to provide the staff of metallographic laboratories with concentrated and precise information about specific materials and their application.    
 