Materialographic Preparation of Human Teeth for Microtensile Testing

​Dental composities are critical to restoring form and function to dental patients around the world. Learn more about the sample preparation for microtensile testing in order to quantify bond strength between the tooth and dental composite.

Watch webinar

Grabación de seminario web

Materialographic Preparation of Human Teeth for Microtensile Testing

​Dental composities are critical to restoring form and function to dental patients around the world. Learn more about the sample preparation for microtensile testing in order to quantify bond strength between the tooth and dental composite.

Microtensile bond testing is used to quantify the bond strength between the dental composite and tooth. In order to perform microtensile testing, the tooth and dental composite must be sectioned into very small tensile samples. Learn how to prepare these samples for microtensile testing.

Información

  • Tema
  • Idioma

    Inglés

  • Disponibilidad

Hora y lugar

Información adicional