How to do efficient materialographic polishing

Improve contrast and planeness by selection of polishing surface.

Watch webinar

Aufgezeichnetes Webinar

How to do efficient materialographic polishing

Improve contrast and planeness by selection of polishing surface.

Is planeness, edge retention or contrast the goal for the preparation? How are the most suitable polishing cloths chosen for the job to be done?


The dynamics of fine grinding and polishing are the basis for understanding how the different polishing surfaces works depending on the sample material. This Webinar will review the basic theory and with examples show how surface characteristics influence the polishing result.